Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Testing and Inspection of Cast Steel Parts for Spherical Bearings: A Complete Technical Guide

Spherical bearing cast steel parts testing is a critical quality control process that verifies the chemical composition, mechanical properties, dimensional accuracy, and internal soundness of cast steel components used in bridge spherical bearings. This technical guide explains the main sample types, testing items, testing methods, applicable standards, and common questions related to spherical bearing cast steel inspection, helping manufacturers, engineering contractors, and supervision units ensure structural safety and compliance with GB/T, ISO, ASTM, and EN requirements.

Technical Overview

Spherical bearings (spherical plane bearings) are widely used load-transfer devices in highway bridges, railway bridges, and large-span steel structures. They carry vertical loads from the superstructure to the substructure while accommodating rotation in all directions through a spherical sliding surface and, in movable types, unidirectional or bidirectional translation. The primary load-bearing components of these bearings, including the upper plate, sphere plates, and base plate, are typically manufactured as steel castings because of their complex geometry and high strength requirements.

Cast steel components are inherently susceptible to solidification defects such as shrinkage cavities, gas porosity, sand and slag inclusions, hot tears, cold shuts, and cracks. Any of these discontinuities, together with deviations in chemical composition, heat treatment condition, or dimensional accuracy, can significantly reduce the load capacity, rotation performance, and service life of the bearing. Therefore, systematic testing of spherical bearing cast steel parts is essential before assembly and installation. Common material grades include ZG270-500 cast carbon steel and G20Mn5 low-temperature cast steel, and the inspection program is generally governed by standards such as GB/T 17955, GB/T 11352, ISO 4990, ASTM A27/A27M, ASTM A781/A781M, and EN 10293. Accredited third-party laboratories routinely perform these evaluations to provide independent verification for project acceptance.

Testing Samples

The scope of spherical bearing cast steel inspection covers all cast components within the bearing assembly, as well as representative test coupons produced under the same conditions.

Upper Bearing Plate (Convex Sphere Plate)

The upper plate integrates the convex spherical surface that defines the rotation center of the bearing. Testing focuses on the integrity of the thick transition sections, the accuracy of the sphere radius, and the surface quality of the sphere seat, since even minor defects on the convex surface can accelerate wear of the sliding material and impair rotational performance.

Intermediate Concave Sphere Plate

The concave intermediate plate works in conjunction with the convex plate and the stainless steel sliding sheet or PTFE interface. Inspection addresses the sphericity of the concave surface, wall thickness uniformity, and internal soundness of the rim areas, which experience concentrated stresses during rotation under load.

Lower Base Plate

The base plate transmits the full bearing reaction into the pier or abutment through anchor bolts and mortar pads. Its cast body, ribs, and bolt-hole bosses are examined for internal discontinuities and for compliance with the planar tolerances that govern load distribution.

Auxiliary and Fixing Components

Guides, side stops, limiting blocks, and other cast steel accessories used in unidirectional and fixed spherical bearings are also inspected, together with separately cast or attached test coupons (keel blocks) that are heat treated in the same furnace load as the production castings.

Testing Items

A complete inspection program for spherical bearing cast steel parts typically includes the following items, with the exact scope defined by the design drawings, the applicable product standard, and the project specification.

  • Chemical composition analysis of carbon, silicon, manganese, phosphorus, sulfur, chromium, nickel, molybdenum, copper, and residual elements
  • Tensile testing to determine yield strength, tensile strength, elongation after fracture, and reduction of area
  • Charpy V-notch impact testing, including low-temperature impact energy at −20 °C or −40 °C for cold-region applications
  • Brinell hardness testing for strength correlation and uniformity verification
  • Ultrasonic testing (UT) for internal defects such as shrinkage, porosity, and inclusions
  • Magnetic particle testing (MT) for surface and near-surface cracks
  • Liquid penetrant testing (PT) for surface defects at accessible locations and on non-magnetic regions
  • Radiographic testing (RT) for designated critical zones where volumetric records are required
  • Visual inspection of surface quality, including cracks, sand burn-on, cold shuts, misruns, and repair weld condition
  • Dimensional and geometric verification, including sphere diameter, sphericity, coaxiality, plate height, bolt-hole position, and surface roughness of the sphere surface
  • Metallographic examination of microstructure and grain size to confirm the effectiveness of normalization, quenching and tempering, or annealing treatments
  • Anti-corrosion coating inspection, including dry film thickness and adhesion of painted or zinc-coated machined surfaces where applicable
  • Repair welding procedure verification, including welder qualification, preheat control, and post-weld NDT re-examination

Testing Methods

Chemical Composition Analysis

Chemical analysis is performed by spark discharge optical emission spectrometry in accordance with GB/T 4336, ASTM E415, or ISO 14707-related laboratory procedures, supplemented by combustion infrared and titrimetric methods for carbon and sulfur when referee results are required. Sampling is normally taken from the material analysis sample poured with each heat, and results must fall within the specified ranges of GB/T 11352, EN 10293, or the equivalent material standard.

Tensile, Impact, and Hardness Testing

Tensile tests are carried out on machined specimens taken from separately cast or attached test coupons that have been heat treated together with the castings, following GB/T 228.1, ASTM E8/E8M, or ISO 6892-1. For ZG270-500, typical acceptance values are a yield strength of at least 270 MPa, a tensile strength of at least 500 MPa, and an elongation of at least 18 percent. Charpy V-notch impact testing is conducted per GB/T 229, ISO 148-1, or ASTM E23, with low-temperature energy requirements applied to G20Mn5 castings used in cold environments. Brinell hardness is measured according to GB/T 231.1, ASTM E10, or ISO 6506 to verify uniformity across the casting.

Ultrasonic Testing

Ultrasonic examination of the casting body is performed with straight-beam and, where geometry requires, angle-beam techniques in accordance with GB/T 7233, ISO 4992, or ASTM A609/A609M. Critical zones, such as the sphere root areas, load-transfer sections, and bolt-hole ligaments, are usually held to a higher quality level, and indications are evaluated against the specified acceptance level for area, length, and amplitude of discontinuities.

Magnetic Particle and Penetrant Testing

Magnetic particle testing per GB/T 9444, ISO 4987, or ASTM E709 is applied to all accessible ferromagnetic surfaces after final machining to detect surface and near-surface cracks, hot tears, and grind marks. Liquid penetrant testing per ISO 3452-1 or ASTM E165 is used for localized areas where magnetic particle techniques are impractical. Relevant linear indications such as cracks are normally cause for rejection unless qualified repair and re-examination procedures are implemented.

Radiographic Testing

Where volumetric documentation is specified, radiographic testing is performed on designated sections according to GB/T 9443, ISO 4993, or ASTM E446 reference radiograph comparison. Digital radiography is increasingly used to shorten examination time while maintaining defect detection sensitivity comparable to film-based techniques.

Dimensional and Geometric Verification

Dimensional inspection verifies overall size, height, bolt-hole diameter and position, and the flatness of mounting surfaces using calibrated instruments and coordinate measuring machines. The spherical surfaces are checked with spherometers, radius templates, or CMM scanning to confirm the sphere radius, sphericity tolerance, and surface roughness, since these parameters directly control rotation torque and contact stress distribution with the sliding interface.

Applications

Testing of spherical bearing cast steel parts serves multiple stages of a project life cycle and supports both manufacturing quality assurance and engineering acceptance.

  • Factory acceptance testing of new spherical bearings for highway and railway bridge construction projects
  • Quality verification of cast steel plates for large-span continuous beam, cable-stayed, and suspension bridges with high vertical loads and large rotation demands
  • Inspection of bearings for municipal elevated roads, interchanges, and rail transit viaducts, including low-temperature grades for cold-climate regions
  • Third-party verification testing requested by owners, general contractors, and supervision engineers before installation
  • In-service condition assessment and failure analysis of bearings during bridge maintenance, renovation, and bearing replacement programs
  • Supplier qualification audits comparing heat-to-heat consistency, heat treatment stability, and repair-welding control across foundries

FAQ

What materials are commonly used for spherical bearing cast steel parts?

The most widely used grades are ZG270-500 cast carbon steel per GB/T 11352 for conventional service and G20Mn5 low-temperature cast steel for regions requiring impact toughness at temperatures as low as −40 °C. Equivalent international materials include castings supplied to ASTM A27, ASTM A781, and EN 10293. The material grade is selected based on design load, ambient temperature, and the ductility requirements of the applicable bearing product standard such as GB/T 17955.

Why is non-destructive testing so important for these castings?

Thick-walled castings are prone to internal shrinkage and gas porosity that cannot be detected visually but can propagate under cyclic bridge loads. Ultrasonic testing reveals internal discontinuities, magnetic particle and penetrant testing reveal surface cracks, and radiographic testing provides volumetric evidence in critical zones. Together, these methods confirm that the casting integrity matches the quality level assumed in the structural design.

How are mechanical property test samples obtained?

Tensile and impact specimens are machined from test coupons cast separately or attached to the production casting and heat treated in the same furnace batch. This approach, required by GB/T 11352 and ISO 4990, ensures that the coupon properties represent the actual metallurgical condition delivered to site. Retest rules allow duplicate testing when a single result falls marginally below the specified value.

What acceptance level is typically applied for ultrasonic testing?

The required quality level depends on the criticality of the zone. Load-bearing sections adjacent to the spherical surfaces and anchor regions are commonly inspected to a stricter quality level, while non-critical machined areas may be held to a moderate level. The applicable level is stated in the design documents or the bearing specification, referencing GB/T 7233, ISO 4992, or ASTM A609 classification.

Can testing be performed on finished bearings or installed bearings?

Yes. On finished assemblies, laboratories verify component markings, material certificates, dimensional fit-up, sliding-surface condition, and coating quality. For installed bearings, in-service inspection addresses corrosion, deformation, fastener condition, and displacement behavior, and non-destructive methods can be applied to accessible cast surfaces without dismantling the structure.

How long does a typical testing program take?

Chemical analysis and mechanical testing of a standard batch are usually completed within several working days once heat-treated coupons are available, while comprehensive NDT of multiple castings depends on size, complexity, and the number of designated inspection zones. Accelerated schedules can generally be arranged with accredited third-party laboratories when project milestones require rapid reporting.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing